Ubicación: Global + English
Global Global Algérie Français Algeria English Angola Português Angola English Argentina Español Argentina English Australia English Austria Deutsch Austria English Azerbaijan English Azerbaijan Русский Bahrain English Bangladesh English Belgium English Belgium Français Belgium Nederlands Brazil Português Brazil English Bulgaria български Bulgaria English Cameroon English Cameroon Français Canada English Canada Français Chile Español Chile English China 中文 China 日本語 China English Colombia Español Colombia English Croatia English Czech Republic Čeština Czech Republic English Denmark English Djibouti English Ecuador Español Ecuador English Egypt English Estonia English Ethiopia English Finland Suomi Finland English France Français France English Georgia English Georgia Русский Germany Deutsch Germany English Ghana English Greece Ελληνικά Greece English Guatemala Español Guatemala English Hong Kong, China English Hong Kong, China 中文 Hungary Magyar Hungary English India English Indonesia English Iraq English Ireland English Italy Italiano Italy English Ivory Coast Français Ivory Coast English Japan 日本語 Japan English Jordan English Kazakhstan Русский Kazakhstan English Kenya English Kuwait English Kyrgyzstan Русский Kyrgyzstan English Latvia English Lithuania English Malaysia English Mauritius English Mauritius français (Maurice) Mexico Español Mexico English Moldova Română Moldova English Mongolia English Morocco English Morocco Français Mozambique Português Mozambique English Netherlands Nederlands Netherlands English New Zealand English Nigeria English Norway English Oman English Pakistan English Paraguay Español Paraguay English Peru Español Peru English Philippines English Poland Polski Poland English Portugal Português Portugal English Qatar English Republic of Korea 한국어 Republic of Korea English Romania Română Romania English Saudi Arabia English Serbia Српски Serbia English Singapore English Slovakia English Slovenia English South Africa English Spain English Spain Español Sri Lanka English Sweden English Switzerland Deutsch Switzerland Français Switzerland Italiano Switzerland English Tanzania English Thailand ไทย Thailand English Togo English Togo Français Tunisia English Tunisia Français Türkiye Türkçe Türkiye English Turkmenistan Русский Turkmenistan English Ukraine Українська Ukraine English United Arab Emirates English United Kingdom English Uruguay Español Uruguay English USA English Uzbekistan English Uzbekistan Русский Vietnam Tiếng Việt Vietnam English

D90 particle size analysis is a critical metric used to quantify the coarse fraction of a particulate material, indicating that 90 percent of the particles are smaller than a specific diameter. This technical guide explores the experimental principles, methodologies, and significance of D90 determination for quality control and research applications. Understanding the D90 value is essential for predicting material behavior in processes ranging from additive manufacturing to pharmaceutical formulation.

D90

Technical Overview

The D90 particle size analysis experiment is designed to determine the particle size distribution of a sample, specifically focusing on the D90 value. The D90 represents the particle diameter where 90 percent of the particles in the sample are smaller. This parameter is a vital indicator of the coarse end of the particle size distribution and is often used to define the upper limit of particle size for quality control specifications.

In a typical cumulative distribution curve, the horizontal axis represents the particle size, while the vertical axis represents the cumulative percentage of particles. The D90 value is read from the curve corresponding to the 90 percent mark. Accurate determination of this value is crucial for ensuring product consistency, as the presence of oversized particles can significantly impact material performance.

Testing Samples

Metal Powders

Metal powders used in additive manufacturing (3D printing) and powder metallurgy are frequently analyzed. The D90 value ensures that the powder does not contain large particles that could clog recoating blades or create defects in the final sintered part.

Ceramic Materials

Ceramic slurries and dry powders are tested to control packing density and sintering behavior. A high D90 value might indicate insufficient milling, leading to porous or weak final products.

Pharmaceutical Powders

Active pharmaceutical ingredients (APIs) and excipients require strict particle size control. The D90 value affects dissolution rates and bioavailability, making it a critical quality attribute for drug manufacturing.

Testing Items

The primary objective of the D90 analysis is to characterize the particle size distribution. The specific testing items include:

  • D10: The particle diameter where 10 percent of the distribution is smaller.
  • D50: The median particle diameter where 50 percent of the distribution is smaller.
  • D90: The particle diameter where 90 percent of the distribution is smaller.
  • Span: A calculation indicating the width of the distribution, defined as (D90 - D10) / D50.

Testing Methods

Laser Diffraction Method

Laser diffraction is the most widely used method for D90 analysis. It operates on the principle that particles scatter light at different angles depending on their size. Large particles scatter light at narrow angles, while small particles scatter light at wide angles. The instrument measures the scattering pattern and calculates the particle size distribution using optical models. This method offers a wide measurement range and high reproducibility.

Sieve Analysis

For larger particle sizes, traditional sieve analysis may be employed. The sample is passed through a stack of sieves with decreasing mesh sizes. The mass retained on each sieve is weighed to determine the particle size distribution. While effective for larger particles, this method is less precise for fine powders and cannot easily generate a continuous D90 curve.

Sedimentation Method

This method determines particle size by measuring the rate at which particles settle in a fluid. It is suitable for materials with densities significantly different from the suspension medium but is generally slower than laser diffraction.

Applications

The D90 particle size analysis experiment serves various critical functions across multiple industries:

  • Quality Control: Ensuring raw materials meet strict specifications before production begins.
  • Process Optimization: Monitoring milling and grinding processes to determine when the target fineness has been achieved.
  • Product Performance: predicting flowability, packing density, and reactivity of powders.
  • Safety Assessment: Evaluating dust hazards where fine particles may pose explosion risks or respiratory hazards.

FAQ

What does a high D90 value indicate?

A high D90 value indicates that a significant portion of the sample consists of large particles. This usually suggests that the material contains coarse aggregates or agglomerates, which may require further milling or screening.

Why is D90 more important than D50 in some industries?

While D50 indicates the average particle size, D90 is often more critical for filtration processes or surface finish applications. Even a small percentage of oversized particles (reflected by the D90) can clog filters, damage spray nozzles, or create surface defects.

How should samples be prepared for the experiment?

Samples must be representative of the bulk material. For dry dispersion methods, care must be taken to avoid agglomeration. For wet dispersion methods, a suitable dispersant must be selected to ensure particles are fully separated without dissolving.